EN 10277-2:2008 standard
W.NR.: 1.0543
Non-alloy steel for structural purposes
heat analysis according to the EN 10277-2:2008 standard
C % | Si % | Mn % | P % | S % | N % | Cu % | |
From | – | – | – | – | – | – | – |
To | – | – | – | 0,045 | 0,045 | 0,012 | – |
according to the EN 10277-2:2008 standard
Thickness mm | Rolled + peeled rolled ( +SH ) |
Cold drawn | |||
( +C ) | |||||
hardness HB | Rm (MPa) | Rp0,2 minimum | Rm (MPa) | A5 % | |
(MPa) | minimum | ||||
≥5≤10 | 540 | da 700 a 1050 | 5 | ||
>10≤16 | 480 | da 680 a 970 | 6 | ||
>16≤40 | da 169 a 211 | da 570 a 710 | 390 | da 640 a 930 | 7 |
>40≤63 | da 169 a 211 | da 570 a 710 | 340 | da 620 a 870 | 8 |
>63≤100 | da 169 a 211 | da 570 a 710 | 295 | da 570 a 810 | 8 |
* Delivery condition: as rolled.
Weldability:
Failing any prescriptions concerning chemical composition, no technical data about this steel weldability are available.
Notes:
CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):
EN 10025-2:2019 | EN 10025:90 | UNI 7070 | DIN 17 100 | NF A35-501 |
E335 | Fe 590-2 | Fe 590 | St 60-2 | A 60-2 |