cold drawn EN 10277:2018 standard
W.NR.: 1.7225
Special alloy steel
analysis according to the EN ISO 683-2:2018 standard
C % | Si % | Mn % | P % | S % | Cr % | Mo % | Cu % | |
From | 0,38 | 0,10 | 0,60 | – | – | 0,90 | 0,15 | – |
To | 0,45 | 0,40 | 0,90 | 0,025 | 0,035 | 1,20 | 0,30 | 0,40 |
according to the EN 10277:2018 standard
Thickness mm |
Annealed + cold drawn ( +A+C ) |
hardness HB max | |
≥5≤10 | 300 |
>10≤16 | 290 |
>16≤40 | 285 |
>40≤63 | 280 |
>63≤100 | 280 |
* Delivery condition: soft annealed.
Weldability:
Bad weldability due to the high crack danger.
Hardenability:
Medium-good hardenability, suitable for hot purposes till a temperature of 500°.
It can be hardened in oil.
Notes:
CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):
UNI 7845 | DIN 17200 | AFNOR 35-552 | AISI-SAE |
42CrMo4 | 42CrMo4 | 42CD4 | 4140 |