EN 10277-2:2008 standard
W.NR.: 1.0401
Non-alloy steel for general purposes
heat analysis according to the EN 10277-2:2008 standard
C % | Si % | Mn % | P % | S % | |
From | 0,12 | – | 0,30 | – | – |
To | 0,18 | 0,40 | 0,80 | 0,045 | 0,045 |
according to the EN 10277-2:2008 standard
Thickness mm |
Rolled + peeled rolled ( +SH ) |
Cold drawn ( +C ) |
|||
hardness HB | Rm (MPa) | Rp0,2 minimum | Rm (MPa) | A5 % | |
(MPa) | minimum | ||||
≥5≤10 | 380 | da 500 a 800 | 7 | ||
>10≤16 | 340 | da 480 a 780 | 8 | ||
>16≤40 | da 98 a 178 | da 330 a 600 | 280 | da 430 a 730 | 9 |
>40≤63 | da 98 a 178 | da 330 a 600 | 240 | da 380 a 670 | 11 |
>63≤100 | da 98 a 178 | da 330 a 600 | 215 | da 340 a 600 | 12 |
* Delivery condition: as rolled.
Weldability:
It is a soft carbon-steel, easily cold machinable and weldable without any particular precautions.
Improved machinability:
Upon request it can be supplied with improved machinability with Pb (lead) addition, for example
Pb=0,15%÷0,35%
Notes:
CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):
UNI 7846 | DIN 17210 | AFNOR 35-551 |
C15 | CK15 | XC12 |