EN 10277-2:2008 standard
W.NR.: 1.0533
Non-alloy steel for structural purposes
heat analysis according to the EN 10277-2:2008 standard
C % | Si % | Mn % | P % | S % | N % | Cu % | |
From | – | – | – | – | – | – | – |
To | – | – | – | 0,045 | 0,045 | 0,012 | – |
according to the EN 10277-2:2008 standard
Thickness mm | Rolled + peeled rolled ( +SH ) |
Cold drawn ( +C ) |
|||
hardness HB | Rm (MPa) | Rp0,2 minimum | Rm (MPa) | A5 % | |
(MPa) | minimum | ||||
≥5≤10 | 510 | da 650 a 950 | 6 | ||
>10≤16 | 420 | da 600 a 900 | 7 | ||
>16≤40 | da 140 a 181 | da 470 a 610 | 320 | da 550 a 850 | 8 |
>40≤63 | da 140 a 181 | da 470 a 610 | 300 | da 520 a 770 | 9 |
>63≤100 | da 140 a 181 | da 470 a 610 | 255 | da 470 a 740 | 9 |
* Delivery condition: as rolled.
Weldability:
Failing any prescriptions concerning chemical composition, no technical data about this steel weldability are available.
Notes:
CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):
EN 10025-2:2019 | EN 10025:90 | UNI 7070 | DIN 17 100 | NF A35-501 |
E295 | Fe 490-2 | Fe 490 | St 50-2 | A 50-2 |