EN 10277:2018 standard

W.NR.: 1.0579

Non-alloy steel for structural purposes

heat analysis according to the EN 10025-2:2019 standard

* P and S = max. 0,030% for long products

                     C % Si % Mn % *P % *S % N % Cu %
     per spessori in mm
 ≤40                                  >40
From
To 0,20 0,22 0,55 1,60 0,025 0,025 0,55

according to the EN 10277:2018 standard

Thickness mm Rolled + peeled rolled
( +SH )
Cold drawn
( +C )
hardness HB Rm (MPa) Rp0,2  minimum Rm (MPa) A5 %
(MPa) minimum
≥5≤10 520 da 630 a 950 6
>10≤16 450 da 580 a 880 7
>16≤40 da 140 a 187 da 470 a 630 350 da 530 a 850 8
>40≤63 da 140 a 187 da 470 a 630 335 da 500 a 770 9
>63≤100 da 140 a 187 da 470 a 630 315 da 470 a 740 9

* Delivery condition: as rolled.

Calcolo del carbonio equivalente:

mn6Cr+Mo+V 5Ni+Cu 15

Weldability:
This steel grade is generally suitable to welding.
Notes:
CORRESPONDENCE WITH OTHER STANDARDS (purely as an indication):

 

EN 10277-2:2008 UNI 7070 DIN 17 100 BS 4360
 S355J2C  Fe 510 D  St 52-3 N  50 D8